牌号简介 About |
---|
全水解级Mowiol和Kuraray Poval是Kuraray销售的聚乙烯醇的商品名。这些是由聚醋酸乙烯酯通过醇解使用连续工艺制造。通过改变聚醋酸乙烯的聚合程度及其水解程度(皂化),可以提供许多不同的等级。我们的pvoh类型以高标准纯度提供,特别是“低灰份和VOC含量”。 Fully hydrolysed grade Mowiol® and Kuraray Poval® are the trade name of the polyvinyl alcohols marketed by Kuraray. These are manufactured from polyvinyl acetate by alcoholysis using a continuous process. By varying the degree of polymerization of the polyvinyl acetate and its degree of hydrolysis (saponification), a number of different grades can be supplied. Our PVOH types are offered in a high standard purity showing especially "low ash and VOC contents". |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表观密度 Apparent density |
0.40 到 0.60 | g/cm³ | DIN 53466 |
溶液粘度 Solution viscosity 2 |
5 到 7 | mPa·s | DIN 53015 |
pH值 PH value 3 |
4.5 到 7.0 | DIN 19261 | |
灰份含量 Ash Content 4 |
< 0.50 | % | |
酯含量 Ester content |
15.0 到 25.0 | mg KOH/g | DIN 53401 |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Degree of Hydrolysis Degree of Hydrolysis 5 |
% | ||
Residual Acetyl Content Residual Acetyl Content |
% | ||
不挥发物含量 nonvolatile content 6 |
% | DIN 53189 | |
甲醇可萃取 Methanol extractable |
% |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 4 % aqueous solution at 20 °C |
3 4 % solution in distilled water |
4 Calculated as Na2O |
5 Saponification |
6 After 3 hours' drying at 105 °C |
【新闻资讯】查看全部
修建节能保温势在必行 聚氨酯、岩棉将直承受益
2016-04-19 北方的许多建筑外墙必须加一层保温板。目前建筑用的保温板多为钢板内夹岩棉或聚苯乙烯泡沫,而目前世界上应用效果综合评价最好的保温板是聚氨酯泡沫作为夹心层的保温板。 聚氨酯保温材料将凭借其低能耗、加工方便、保温效果极佳等诸多优势,在未来很长一个阶段里聚氨酯保温材料将引领中国的保温建材市场。外墙能耗占建筑节能的30%左右,外墙外保温已成为重中之重。在诸多外墙保温材料中,聚氨酯综合性能最佳,已在国外得到大量应用。岩棉则在高防火要求领域占据一席之地。岩棉等无机材料需求大幅增长,但201 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |