牌号简介 About |
---|
TATREN® HT 3 06是一种具有良好加工稳定性的均聚物,可以大批量加工。这种级别的添加剂包装在胶带生产过程中提供了低水携带。TATREN® HT 3 06具有极高的机械性能和高刚度。应用TATREN® HT 3 06用于生产高强度编织带和单丝。适用于生产大袋、地毯衬垫、绳索及船用绳索、绳线等的聚丙烯织物,也可用于挤出、片材挤出及热成型、注塑及复合。TATREN® HT 3 06适用于食品接触。产品符合食品接触法规。该等级适用于制药包装产品的生产。 TATREN HT 3 06 is homopolymer of good processing stability and it can be processed at high throughput. Additive package of this grade provides low water carry over during production of tapes. TATREN HT 3 06 is characterised by exceptionally high mechanical properties and high stiffness. Applications TATREN HT 3 06 is intended for production of high tenacity weaving tapes and monofilaments. It is well suitable to produce PP fabrics for big-bags production, carpet backing, ropes and marine ropes, twines etc. This grade can be used also for extrusion, sheet extrusion and thermoforming, injection moulding and compounding. TATREN HT 3 06 is suitable for food contact. The product complies with Food Contact Regulations. The grade is suitable for manufacturing of pharmaceutical packing-product. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,2.16kg 230℃,2.16kg |
3.0 | g/10min | ISO 1133 |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
23℃,注塑成型 23 ℃, injection molding |
6.0 | kJ/m² | ISO 180-A |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
110 | ℃ | ISO 75-2/B |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
注塑成型 injection molding |
1800 | MPa | ISO 527-2 |
拉伸强度 tensile strength |
|||
屈服,注塑成型 Yield, injection molding |
36.0 | MPa | ISO 527-2 |
拉伸应变 Tensile strain |
|||
屈服,注塑成型 Yield, injection molding |
% | ISO 527-2 | |
弯曲模量 Bending modulus |
|||
注塑成型 injection molding |
MPa | ISO 178 | |
洛氏硬度 Rockwell hardness |
|||
R 级 R-level |
ISO 2039-2 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
【干货】玻纤增强塑料注射成型时出现浮纤的解决方法
2020-11-14 搜料网资讯: 玻纤增强塑料注射成型时,各机构运行基本正常,但制品出现了比较严重的外观质量问题,表面产生了放射状的白色痕迹,而且这种白色痕迹随玻纤含量的增加趋于严重, |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |