牌号简介 About |
---|
聚苯硫醚(PPS)是一种热塑性薄膜,具有优异的耐化学性和良好的电、物理性能。 Polyphenylene sulfide, PPS, is a thermoplastic film that has excellent chemical resistance and good electrical and physical properties. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.35 | g/cm³ | ASTM D792 |
吸水率 Water absorption rate |
|||
24hr 24hr |
0.020 | % | ASTM D570 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
75 | µm | |
割线模量 Secant modulus |
|||
MD MD |
2370 | MPa | ASTM D882 |
拉伸强度 tensile strength |
|||
MD,断裂 MD, fracture |
46.9 | MPa | ASTM D882 |
拉伸应变 Tensile strain |
ASTM D882 | ||
MD,屈服 MD, yield |
% | ASTM D882 | |
MD,断裂 MD, fracture |
% | ASTM D882 | |
落锤冲击 Drop hammer impact |
g | ASTM D1709 | |
面积系数 Area coefficient |
ft²/lb/mil | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
玻璃化转变温度 Glass transition temperature |
℃ | ASTM D3418 | |
熔融峰值温度 Melting peak temperature |
℃ | ASTM D3418 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
介电强度 Dielectric strength |
|||
0.1 mm 0.1 mm |
kV/mm | ASTM D149 | |
介电常数 Dielectric constant |
|||
1 kHz 1 kHz |
ASTM D150 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
极限氧指数 Extreme oxygen index |
% | ASTM D2863 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
利安德巴塞尔的最新分子回收中试车间正式投运
2020-09-09 搜料网资讯:9月8日,全球最大的塑料、化工和炼油公司之一利安德巴塞尔宣布,该公司在其意大利费拉拉基地建造的MoReTec分子回收车间正式投运。新设施将运用利安德巴塞尔专有的 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |