牌号简介 About |
---|
氟橡胶,90-98°IRHD。偏氟乙烯、六氟丙烯和四氟乙烯三元共聚物。为满足ASTM D2000的要求,请拨打M3HK914、A1-10、B37、B38、EF31、EO78、Z1。其中,z1=硬度90-98。ASTM名称=FKM。ISO名称=FPM。一种坚硬的抗挤压橡胶,专门设计用于高压应用。在高温下具有优异的耐油、耐燃料和耐液压油性能。 Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Where Z1 = hardness 90-98. ASTM designation = FKM. ISO designation = FPM. A hard, anti-extrusion resistant rubber, specially designed for use in high pressure applications. Excellent resistance to oils, fuels and hydraulic fluids at high temperature. |
技术参数 Technical Data | |||
---|---|---|---|
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
IRHD 硬度 IRHD hardness |
95 | ASTM D1415 , ISO 48 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服 yield |
15.0 | MPa | ASTM D412 , ISO 37 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
100 | % | ASTM D412,ISO 37 |
压缩形变 Compression deformation |
|||
200℃,24 hr 200℃,24 hr |
25 | % | ASTM D395,ISO 815 |
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
空气中拉伸强度的变化率 The rate of change in tensile strength in air |
|||
250℃,72 hr 250℃,72 hr |
-10 | % | ASTM D412 , ISO 37 |
空气中极限伸长率的变化率 The rate of change in ultimate elongation in air |
|||
250℃,72 hr 250℃,72 hr |
% | ASTM D412 , ISO 37 | |
空气中 IRHD 硬度的变化率 The change rate of IRHD hardness in the air |
|||
250℃,72 hr 250℃,72 hr |
ASTM D573 , ISO 188 | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
最高工作温度 Maximum operating temperature |
℃ |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
先行指标“剧透”我国外贸开局良好 将继续拉动经济强劲增长
2022-02-15 集装箱整齐排列、拖车有序通行、汽笛声起起伏伏,深圳盐田港春节以来格外繁忙。据深圳海关统计,春节以来(1月31日2月9日),盐田港吞吐量达44.9万标箱,经此进出口的货物达53. |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |