牌号简介 About |
---|
改性聚烯烃包括改性聚乙烯和改性聚丙烯。改性聚乙烯主要用于电缆护套。黑色聚乙烯化合物由聚乙烯树脂、炭黑、抗氧化剂等组成。黑色聚乙烯化合物适用于通信电缆、控制电缆、信号电缆、电力电缆、光缆、海底电缆等。符合GB15065-94标准。改性聚丙烯包括阻燃、玻璃纤维和矿物增强耐候等,广泛应用于电子电器、家用电器、汽车配件、灯具、机械元器件和插座等。此外,我们还根据客户的具体要求开发新产品。阻燃PP特性:阻燃PP应用:电器配件、照明配件、风扇、电源插座、电气螺栓 SlLVER® Modified Polyolefin includes modified polyethylene and modified polypropylene. Modified polyethylene is mainly applied to cable jacket. Black polyethylene compound is composed of polyethylene resin,carbon black, antioxidant and so on. Black polyehylene compound is applied to communication cable,contoll cable,signal cable,power cable,optical cable and submarine cable. It conforms to GB15065-94 Standard. Modified PP including flame resistant, glass fiber and mineral reinforced and weather—resistant, is widely applied in electronic & electrical appliances, household appliances, auto accessories, lightings, mechanical components and sockets, and so on. In addition, we develop new products according to customer's specific requirements. Flame retardant PP Characteristics: flame retardance PP Applications: electric appliance fittings, lighting accessory, fan, electric outlet and electric bolt |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.978 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,2.16kg 230℃,2.16kg |
10 | g/10min | ASTM D1238 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength 2 |
30.0 | MPa | ASTM D638 |
拉伸应变 Tensile strain 2 |
|||
断裂 fracture 2 |
> 200 | % | ASTM D638 |
弯曲模量 Bending modulus 3 |
1300 | MPa | ASTM D790 |
弯曲强度 bending strength 3 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
23℃ 23℃ |
kJ/m² | ASTM D256 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ASTM D648 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
0.80 mm 0.80 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 2.0 in/min |
3 0.20 in/min |
【新闻资讯】查看全部
非标模具零件精加工时应该如何操控
2016-06-29 一套整个模具由众多模具零件组合而成,而其中非标模具零件直接影响模具的质量,而非标模具零件的质量由精加工来完成。那在非标模具零件精加工时应该如何控制呢? 1、一般模具零件制造企业,精加工一般都是采用磨削、电加工及钳工; 2、模具精加工控制: A:模具非标零件加工,针对不同的材质同的技术要求进行适应性加工,它具有一定的可塑性,可通过对加工的控制,达到好的加工效果; B:根据零件的外观形状不同,大致可把零件分三类:轴类、板类与异形零 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |