牌号简介 About |
---|
Tecnoflon for 532是一种中等粘度固化含氟弹性体共聚物。该等级非常适合需要优良的压缩永久变形和优越的模具释放的应用。它可以配制成符合MIL-R83428B和其他主要氟橡胶规格。Tecnoflon® FOR 532的一些基本性能是:固化速度非常快,良好的防焦安全性,良好的模具流动性,优越的模具释放性,无模具污染,非常低的压缩永久变形,Tecnoflon for 532可用于O型环、垫圈和密封件的压缩和转移成型。该产品可以使用典型的氟弹性体混合配料,混合可以通过两个辊磨机或内部搅拌机完成。这种材料可以挤压成软管或型材,也可以压延成板料或带料。制成品可采用多种橡胶加工方法生产。 TECNOFLON® FOR 532 is a medium viscosity cure incorporated fluoroelastomer copolymer. This grade is well suited for applications where excellent compression set and superior mold release, are required. It can be compounded to meet MIL-R83428B and other major fluoroelastomer specifications. Some of the basic properties of Tecnoflon® FOR 532 are: Very fast cure rate Excellent scorch safety Good mold flow Superior mold release Lack of mold fouling Very low compression set TECNOFLON® FOR 532 can be used for compression and transfer moulding of O-rings, gaskets, and seals. The product can be mixed using typical fluoroelastomers compounding ingredients and mixing can be accomplished with two-roll mills or internal mixers. The material can be extruded into hoses or profiles and can be calendered to make sheet stocks or belting. Finished goods can be produced by a variety of rubber processing methods. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
门尼粘度 Mooney viscosity 2 |
|||
ML 1+10,121℃ ML 1+10,121℃ 2 |
45 | MU | |
氟含量 Fluorine content 2 |
66 | % |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 聚合物原料 |
【新闻资讯】查看全部
腾讯、网易等游戏企业和平台被约谈!回应来了
2021-09-09 搜料网资讯: 9月8日,中央宣传部、国家新闻出版署有关负责人会同中央网信办、文化和旅游部等部门,对腾讯、网易等重点网络游戏企业和游戏账号租售平台、游戏直播平台进行约谈 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |