型号:EstaGrip® ST 80A TPE是80A聚醚型热塑性聚氨酯。特点:硬度低,手感柔软,握力好;优异的粘合性用途:注塑-二次成型 Type: EstaGrip® ST 80A TPE is an 80A Polyether-Type Thermoplastic Polyurethane. Features: Low durometer soft feel for excellent grip; outstanding adhesion Uses: Injection Molding - Overmolding |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.06 | g/cm³ | ASTM D792 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
ASTM D412 | ||
断裂,0.762 mm Fracture, 0.762 mm |
22.8 | MPa | ASTM D412 |
100% 应变,0.762 mm 100% strain, 0.762 mm |
3.70 | MPa | ASTM D412 |
300% 应变,0.762 mm 300% strain, 0.762 mm |
6.70 | MPa | ASTM D412 |
拉伸应变 Tensile strain |
|||
断裂,0.762 mm Fracture, 0.762 mm |
750 | % | ASTM D412 |
撕裂强度 tear strength 2 |
|||
0.762 mm 0.762 mm 2 |
kN/m | ASTM D624 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
玻璃化转变温度 Glass transition temperature |
℃ | DSC | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,5 秒 Shore A, 5 seconds |
ASTM D2240 | ||
泰伯耐磨性 Taber abraser |
|||
1000 周期,1000 g,H-18 转轮 1000 cycles, 1000 g, H-18 wheels |
mg | ASTM D3389 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 C 模具 |
【新闻资讯】查看全部
国务院:原油一次加工能力严控在10亿吨!石化产能利用率80%以上!
2021-10-27 搜料网资讯: 国务院在前两天发布《关于完整准确全面贯彻新发展理念做好碳达峰中和工作的意见》后,紧接着在10月26日,又发布了《国务院关于印发2030年前碳达峰行动方案的通知》 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |