牌号简介 About |
---|
Polytrope Str 3568EU树脂是一种低光泽、耐候、烯烃帽树脂。它是无应力美白,并提供特殊的耐用性,以防凹痕和划痕。它是专门为共挤出工艺设计的,作为一种盖树脂,覆盖在聚变str增强聚烯烃tpo和fr tpo基树脂上。它特别适合热成型应用,因为它通过热成型过程保持浮雕纹理和低光泽。POLYTROPE® STR 3568EU-01 NATURAL容易上色。瓶盖树脂的低光泽和耐用性使其能够匹配或超过其他用于室内和室外的低光泽表面材料的性能和外观。 POLYTROPE STR 3568EU resin is a low gloss, weatherable, olefin cap resin. It is non-stress whitening and provides exceptional durability against denting and scratches. It is specifically designed for the co-extrusion process as a cap resin over POLYTROPE STR enhanced polyolefin TPO and FR TPO base resins. It is especially suited for thermoformed applications, as it maintains embossed texture and low gloss through the thermoforming process. POLYTROPE STR 3568EU-01 NATURAL is easily colored. The low gloss and durability of the cap resin enables it match or exceed the performance and appearance of other low gloss surfacing materials for interior and exterior applications. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.888 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,2.16kg 230℃,2.16kg |
0.60 | g/10min | ISO 1133 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服,23℃ Yield, 23 ℃ |
16.5 | MPa | ISO 527-2 |
拉伸应变 Tensile strain |
|||
断裂,233℃ Fracture, 233 ℃ |
650 | % | ISO 527-2 |
弯曲模量 Bending modulus |
|||
弦,23℃ String, 23 ℃ |
255 | MPa | ISO 178 |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
-40℃,Total Energy,Ductile Failure -40℃,Total Energy,Ductile Failure |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/Bf | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
|||
3.20 mm 3.20 mm |
UL 94 | ||
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
60°,3180 µm,热塑,光滑 60 °, 3180 µ m, thermoplastic, smooth |
ISO 2813 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 方法 A |
3 类型 1, 2,0 in/min |
4 类型1A, 0,079 in/min |
【新闻资讯】查看全部
巴菲特麾下伯克希尔收购朗盛3%股份
2017-05-31 北京时间5月30日晚间消息,据路透社报道,德国化学品生产商朗盛(Lanxess)周一披露信息称,亿万富翁投资者、“股神”沃伦・巴菲特(Warren Buffet)麾下伯克希尔哈撒韦公司(Berkshire Hathaway)已经收购了该公司的3%股份。 受此消息影响,朗盛股价此后上涨2.9%,至65.06欧元。 朗盛在一份监管文件文件中披露信息称,伯克希尔哈撒韦旗下通用再保险公司(General Reinsurance)在5月19日收购了略高于3%的公司股份 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |