牌号简介
Sarlink® TPV X18035是一种高性能热塑性硫化胶,用于汽车和工业应用。Sarlink® TPV X18035是一种低硬度,低密度等级表现出优越的压缩永久性和耐化学性。这一等级可以通过注射成型和挤压加工。 Sarlink TPV X18035 is a high performance thermoplastic vulcanizate used in automotive and industrial applications. Sarlink TPV X18035 is a low hardness, low density grade exhibiting superior compression set and chemical resistance. This grade can be processed by injection molding and extrusion.
Sarlink TPV 3100系列是主要为通用、汽车和工业应用设计的工程材料,需要良好的热、机械和物理性能平衡。sarlink 3135是一种低硬度、低密度、多用途的热塑性硫化胶,可通过注塑、吹塑或挤出加工,适用于夹持器、密封件、垫圈、型材、软管和管、波纹管和其他物品。 SARLINK® TPV 3100 series are engineered materials designed primarily for general purpose, automotive and industrial applications requiring a good balance of thermal, mechanical, and physical properties. SARLINK® 3135, available in NAT and BLK, is a low hardness, low density, multi-purpose thermoplastic vulcanizate that can be processed by injection molding, blow molding or extrusion for applications such as grips, seals, gaskets, profiles, hose & tubes, bellows, and other articles.
产品描述
厂家:
美国特诺尔爱佩斯 Teknor Apex
美国特诺尔爱佩斯 Teknor Apex
类别:
TPV TPV
TPV TPV
填料:
用途:
垫圈,型材,耐候性密封条,汽车的发动机罩下的零件,工业应用,橡胶取代,密封件,插头,隔膜,通用,汽车领域的应用,O型圈,汽车内部零件
密封件,通用,吹塑成型应用,工业应用,垫圈,O型圈,汽车领域的应用,汽车外部零件,汽车内部零件,家电部件,型材,管道密封,把手,汽车的发动机罩下的零件,橡胶取代,插头
性能特点:
易加工,韧性好,弯曲性能好,低硬度,粘结性好,有弹性,低密度,耐化学性 Excellent Processability,Good flexibility,High elastic,Low Hardness,Good bond,Elastic,Low density,Solvent resistance
易加工,韧性好,表面光泽度好,弯曲性能好,耐高温,粘结性好,有弹性,低密度,硬度低,耐化学性,熔体稳定性高,可粘结性,防火阻燃等级HB Excellent Processability,Good flexibility,Good surface appearance,High elastic,High Heat Resistance,Good bond,Elastic,Low density,Low Hardness,Solvent resistance,Higher melt stability,Agglomerability,HB
加工条件:
挤出 Extrusion
注射成型 Injection Molding
技术参数
物理性能 PHYSICAL
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
密度
Density
g/cm³
ASTM D792
密度
Density
g/cm³
ISO 1183
机械性能 MECHANICAL
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
ASTM D2240
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
ISO 868
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
ASTM D2240
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
ISO 868
弹性体 ELASTOMER
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
压缩形变(125℃,70 hr)
Compression deformation
%
压缩形变(125℃,70 hr)
Compression deformation
%
ASTM D395
压缩形变(125℃,70 hr)
Compression deformation
%
ISO 815
压缩形变(23℃,22 hr)
Compression deformation
%
压缩形变(23℃,22 hr)
Compression deformation
%
ASTM D395
压缩形变(23℃,22 hr)
Compression deformation
%
ISO 815
压缩形变(70℃,22 hr)
Compression deformation
%
压缩形变(70℃,22 hr)
Compression deformation
%
ASTM D395
压缩形变(70℃,22 hr)
Compression deformation
%
ISO 815
拉伸应变(TD,断裂)
Tensile strain
%
拉伸应变(断裂)
Tensile strain
%
ASTM D412
拉伸应变(断裂)
Tensile strain
%
ISO 37
拉伸应变(流量,断裂)
Tensile strain
%
拉伸应变(流量,断裂)
Tensile strain
%
ASTM D412
拉伸应变(流量,断裂)
Tensile strain
%
ISO 37
拉伸强度(MD,100% 应变)
tensile strength
MPa
拉伸强度(MD,100% 应变)
tensile strength
MPa
ASTM D412
拉伸强度(MD,100% 应变)
tensile strength
MPa
ISO 37
拉伸强度(MD,断裂)
tensile strength
MPa
拉伸强度(MD,断裂)
tensile strength
MPa
ASTM D412
拉伸强度(MD,断裂)
tensile strength
MPa
ISO 37
拉伸强度(TD,100% 应变)
tensile strength
MPa
拉伸强度(TD,100% 应变)
tensile strength
MPa
ASTM D412
拉伸强度(TD,100% 应变)
tensile strength
MPa
ISO 37
拉伸强度(TD,断裂)
tensile strength
MPa
拉伸强度(断裂)
tensile strength
MPa
ASTM D412
拉伸强度(断裂)
tensile strength
MPa
ISO 37
撕裂强度(TD)
tear strength
kN/m
ASTM D624
撕裂强度(TD)
tear strength
kN/m
ISO 34-1
老化性能 AGING
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
体积变化(125℃,70 hr,in IRM 903 Oil)
Volume change
%
ASTM D471
体积变化(125℃,70 hr,in IRM 903 Oil)
Volume change
%
ISO 1817
体积变化(125℃,70 hr,在IRM 903油中)
Volume change
%
ISO 1817
在空气中断裂时拉伸应力变化 - TD(135℃,1000 hr)
Changes in tensile stress when fractured in air - TD
%
在空气中断裂时拉伸应力变化 - TD(135℃,1000 hr)
Changes in tensile stress when fractured in air - TD
%
ASTM D573
在空气中断裂时拉伸应力变化 - TD(135℃,1000 hr)
Changes in tensile stress when fractured in air - TD
%
ISO 188
在空气中断裂时拉伸应力变化 - TD(150℃,168 hr)
Changes in tensile stress when fractured in air - TD
%
在空气中断裂时拉伸应力变化 - TD(150℃,168 hr)
Changes in tensile stress when fractured in air - TD
%
ASTM D573
在空气中断裂时拉伸应力变化 - TD(150℃,168 hr)
Changes in tensile stress when fractured in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变 135℃,1000 hr)
Change rate of tensile strength in air - TD
%
空气中拉伸强度的变化率 - TD(100% 应变 135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(100% 应变 135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变 150℃,168 hr)
Change rate of tensile strength in air - TD
%
空气中拉伸强度的变化率 - TD(100% 应变 150℃,168 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(100% 应变 150℃,168 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中邵氏硬度的变化率(邵氏 A,135℃,1000 hr)
The rate of change of Shore hardness in air
空气中邵氏硬度的变化率(邵氏 A,135℃,1000 hr)
The rate of change of Shore hardness in air
ASTM D573
空气中邵氏硬度的变化率(邵氏 A,135℃,1000 hr)
The rate of change of Shore hardness in air
ISO 188
空气中邵氏硬度的变化率(邵氏 A,150℃,168 hr)
The rate of change of Shore hardness in air
空气中邵氏硬度的变化率(邵氏 A,150℃,168 hr)
The rate of change of Shore hardness in air
ASTM D573
空气中邵氏硬度的变化率(邵氏 A,150℃,168 hr)
The rate of change of Shore hardness in air
ISO 188
补充信息
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
熔体表观粘度 - Capillary,@ 206/s(200℃)
Apparent viscosity of melt - Capillary, @ 206/s
Pa·s
ASTM D3835
熔体表观粘度 - Capillary,@ 206/s(200℃)
Apparent viscosity of melt - Capillary, @ 206/s
Pa·s
ISO 11443
熔体表观粘度(Capillary,206 1/s,200℃)
Apparent viscosity of melt
Pa·s
ISO 11443
法律声明
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
热性能 THERMAL
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
相对温度指数(冲击机械性能)
Relative temperature index
℃
UL 746
相对温度指数(强度机械性能)
Relative temperature index
℃
UL 746
相对温度指数(电气性能)
Relative temperature index
℃
UL 746
阻燃性能 FLAMMABILITY
Sarlink® TPV X18035
Sarlink® TPV 3135
单位 UNIT
测试方法 TEST METHOD
1.50 mm,所有颜色
1.50 mm, all colors
UL 94