牌号简介 About |
---|
Westlake Hivor聚乙烯LT74104是一种高强度线性低密度聚乙烯,不含防滑块。它是为吹塑应用而设计的,非常适合需要良好冲击和撕裂强度的消费者和工业包装市场。使用USIGN LT74104生产的薄膜缺陷小,便于在较薄的厚度下生产。 WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip of antiblock. It is designed for blown applications and is well suited for consumer and industrial packaging markets which require good impact and tear strength. Films produced usign LT74104 exhibit low imperfections and facilitate production at thinner guages. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.920 | g/cm³ | ASTM D4883 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
1.0 | g/10min | ASTM D1238 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
割线模量 Secant modulus |
|||
1% 正割,TD 1% secant, TD |
241 | MPa | ASTM D882 |
1% 正割,MD 1% secant, MD |
220 | MPa | ASTM D882 |
拉伸强度 tensile strength |
|||
TD,断裂 TD, fracture |
39.0 | MPa | ASTM D882 |
MD,断裂 MD, fracture |
MPa | ASTM D882 | |
拉伸应变 Tensile strain |
|||
TD,断裂 TD, fracture |
% | ASTM D882 | |
MD,断裂 MD, fracture |
% | ASTM D882 | |
落锤冲击 Drop hammer impact |
g | ASTM D1709 | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45° 45° |
ASTM D2457 | ||
雾度 Haze |
% | ASTM D1003 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
OPEC+维持产量计划预期推动 原油期货收盘走高
2022-01-04 搜料网资讯: 北京时间4日凌晨,美国原油期货价格周一收高。市场普遍预计石油输出国组织及其盟友(OPEC+)将在周二的会议上坚持将月度原油产量提高40万桶/日的计划。 以Helima Crof |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |