牌号简介 About |
---|
Neoplast™ 243 HOFR是动态硫化,阻燃热塑性硫化(TPV)基于聚烯烃化学,旨在注塑和挤出应用。主要特点:优良的耐臭氧性、优异的亚零冲击性、符合RoHS标准、阻燃性 Neoplast 243 HOFR is dynamically vulcanized, flame retardant thermoplastic vulcanizate (TPV) based on polyolefin chemistry and is intended for Injection Moulding and Extrusion applications. Key Features: Excellent Ozone resistance, Excellent sub zero impact, RoHS Compliant, flame retardant |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density 2 |
1.10 | g/cm³ | ASTM D792 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 D,23℃,5 秒 Shore D, 23 ℃, 5 seconds |
43 | ASTM D2240 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength 3 |
|||
断裂 fracture 3 |
14.7 | MPa | ASTM D412 |
100% 应变 100% strain 3 |
10.8 | MPa | ASTM D412 |
拉伸应变 Tensile strain 3 |
|||
断裂 fracture 3 |
600 | % | ASTM D412 |
撕裂强度 tear strength 3 |
kN/m | ASTM D624 | |
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
空气中拉伸强度的变化率 The rate of change in tensile strength in air |
|||
150℃,168 hr 150℃,168 hr |
% | ASTM D573 | |
空气中极限伸长率的变化率 The rate of change in ultimate elongation in air |
|||
150℃,168 hr 150℃,168 hr |
% | ASTM D573 | |
空气中硬度计硬度的变化率 The rate of change in hardness of a hardness tester in the air |
|||
150℃,168 hr 150℃,168 hr |
ASTM D573 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 23°C |
3 C 模具, 20 in/min |
【新闻资讯】查看全部
塑料回收行业继续发力,以达到欧盟的目标
2022-05-23 2020年,欧盟27+3国家的塑料回收总装机容量比前一年增加了110万台,其中 欧盟27+3国家包括 欧盟成员国、英国、挪威和瑞士 。新的数据表明,塑料回收行业仍然保持弹性。尽管疫情带来 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |